کلیدواژهها
|
aluminium wire, digoxin, layered double hydroxide, solid-phase microextraction, molecularly
imprinted polymer
|
چکیده
|
Introduction: A new solid-phase microextraction fibre is fabricated through polymerisation of molecularly imprinted polymer on the surface of a layered double hydroxide
framework that has been fabricated via the in situ synthesis on a non-porous anodic
aluminium oxide/aluminium wire as both the substrate and the aluminium source.
Objective: The synthesized SPME fiber was performed to analyze trace digoxin in
real samples.
Material and method: A one-at-a-time optimization strategy was applied for optimizing the important extraction parameters such as extraction solvent, extraction time,
stirring rate, pH, ionic strength, and desorption time.
Result: Aluminum surface before and after anodizing and LDH structure reveal that
anodizing and preparation LDH increases the surface area and adsorption capacity of
aluminum wire.
Conclusion: Under optimum conditions, the repeatability for one fibre (n = 3),
expressed as relative standard deviation (RSD %), was 5.2%
|