مشخصات پژوهش

صفحه نخست /Optimizing Photocatalytic ...
عنوان Optimizing Photocatalytic Efficiency and Durability of Zeolite-Based Catalysts via Cation Doping for Effective Dye Contaminant Remova
نوع پژوهش مقاله چاپ‌شده در مجلات علمی
کلیدواژه‌ها Double-metal decoration, Photodegradation, 4-Nitrophenol, Pseudo-first order, COD
چکیده Ce and Fe decorated on dealuminated zeolite Y (CFDDAZY) framework were prepared using isomorphous substitution method using dealumination treatment and impregnation methods to the formation of Si-O-Ce and Si-O-Fe bonds. For this purpose, we selected three distinct ratios of metals/zeolite, being 1:3, 1:10, and 1:20. An important outcome was achieved with a 1:20 ratio of metals to zeolite, providing strong evidence for the superiority of this configuration. The catalyst was characterized using XRD, FT-IR, UV-Vis, FESEM, TEM, EDX, and BET techniques. The prepared catalyst was evaluated in the degradation of 4-nitrophenol. To optimize the process, we conducted the effect of various parameters, including reaction time, catalyst amount, temperature, pH, isoelectric point, and 4-NP concentration on the photodegradation process. The optimal conditions for the removal of 4-NP were obtained in the presence of DAZY decorated with Fe and Ce under ultraviolet radiation, 40 μL of hydrogen peroxide, 0.03 g of photocatalyst, and a concentration of 5×10-4 M 4-nitrophenol during 90 minutes. The mineralization of 4-nitrophenol (4-NP) was verified through COD experiments, resulting in a removal efficiency of 72.80%. Studying Hinshelwood's equations revealed that the reaction rate was pseudo-first-order. The catalyst can be reused up to five times while maintaining its catalytic activity. Furthermore, the proposed degradation mechanism is introduced.
پژوهشگران مریم موسوی فر (نفر اول)، سارا اکبری (نفر دوم)، مریم نجات دهکردی (نفر سوم)